PVC coating
본문
Application
- Coating PVC compound for marine cable.
Features
- Excellent exterior and flame resistance
- Excellent extrusion and workability
Major physical properties and process temperature
Test Item | UNIT | Value | Test method | |
---|---|---|---|---|
P-40(FX)/LF | ||||
Room Temp. | 상온인장강도 | kgf/㎟ | 1.65 | KS M 3156 |
상온신장율 | % | 276.2 | ||
Aging Test (100℃×168hr) |
가열 후 인장강도 | % | 96.5 | KS M 3156 100℃×240hrs |
가열 후 신장율 | % | 93.2 | ||
Oil Test (70℃×4hr) |
Retention of T/S | % | - | |
Retention of E/L | % | - | ||
LOI | 29 | KS M 3032 | ||
내한성 | ℃ | -18 | KS M 3156 7.6 크렉없을것,-20 |
|
열안정성 | ℃/min | 215 | KS M 3156 7.7 조건:180℃ |
|
비중 | g/㎤ | 1.479 | KS M 0004 | |
경도 | - | 90 | KS M 6518 10초 후 값 |
|
가열감량시험 | 1.25 | IEC 60811-3-2 100℃×168hrs |
||
Application | 선박용 JIS Type 씨즈 |
- Product characteristics shown above are only guidelines not the actual product specification.
- Process temperature conditions for the product may differ according to the technical spec of the machinery and processing condition.