Major physical properties and process temperature
Test Item | UNIT | Value | Test method | ||
---|---|---|---|---|---|
WS-801FR-LF | VZ-2103 | ||||
Room Temp. | Tensile Strength | Mpa | 17 | 16 | IEC-60811 |
Elongation | % | 260 | 260 | ||
Aging Test (100℃×240hrs) |
Retention of T/S | % | 94 | 92 | IEC-60811 |
Retention of E/L | % | 89 | 81 | ||
Specific Gravity | g/㎤ | 1.54 | 1.66 | ASTM D 792 | |
Volume Resistivity at 30℃ | Ω·㎝ | 7.5×10^12 | 4.5×10^12 | ASTM D 257 | |
LOI | 39 | 48 | ASTM D 2863 | ||
Thermal Stability | Hrs | 4:45 | 4:40 | ASTM D 4202 | |
RoHS (Pb, Cr6+ ,Cd, Hg, PBBs, PBDEs,) |
PPM | N.D. | N.D. | XRF | |
Description | CMR급 | CMP급 | |||
Application | Set Indoor, Vertical | Set in the plenum |