Major physical properties and process temperature

Test Item UNIT Test method Spec Value
WS-1004 X WS1004 HS
Tensile Strength Kgf/㎟ ICE 60811-1-1 Min. 1.27 2.50 2.21
Elongation % Min. 200 700 800
Aging Test
(135℃.168hrs)
Retention of Tensile Strength % ICE 60811-1-2 75~125 100 102
Retention of Elongation % 75~125 92 97
Hot Set (200'C, 15min, 20N) Hot % IEC 60811-2-1 Max.175 90 105
Set % Max.15 -5 -2.5
Shrinkage test 130'C 1hr.
Distance La:200mm
% IEC 60811-1-3 Max.4 1 1

Volume Resistivity 

Ω·㎝​ ASTM D 257 Min.1 x 10^15 1.09 x 10^17 -
Packing
  • 500kg Carton Box
  • 25kg Aluminum Bag
Recommended extrusion temperature : unit (℃)
Zone 1 Zone 2 Zone 3 Zone 4 Neck Head Die
160 165 170 175 185 190 210